100% Modulus 0.00248 GPa
0.360 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-265A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00248 GPa
0.360 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00248 GPa
0.360 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2161X Fluoroelastomer  (discontinued **)
Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneMedium viscosityProcess targets: compression and transfer molding, and calenderingProprietary incorporated cure technologyExcell..