Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00202 GPa | 0.293 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
100% Modulus | 0.00202 GPa | 0.293 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00202 GPa | 0.293 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00202 GPa | 0.293 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |