Polymer Property : 100% Modulus = 0.00198 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00198 GPa
0.287 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer
Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited..
100% Modulus 0.00198 GPa
0.287 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer
Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a..