Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00124 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00124 GPa
0.180 ksi
ASTM D412
Huntsman IROGRAN® PS 455-215 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
100% Modulus 0.00124 GPa
0.180 ksi
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
100% Modulus 0.00124 GPa
0.180 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have an excellent soft t..
100% Modulus 0.00124 GPa
0.180 ksi
3M 8440 Silicone Rubber Cold Shrink Connector Insulators
3M™ Cold Shrink Connector Insulators 8440 Series are open ended, silicone rubber, tubular sleeves. The sleeves are factory expanded and assembled on a removable supporting plastic core. Each rubber..
100% Modulus 0.00124 GPa
0.180 ksi
ASTM D412
Advanced Polymer Alloys DuraGrip™ 6840 Thermoplastic Elastomer
With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte..
100% Modulus 0.00124 GPa
0.180 ksi
cured 15 mins @ 150°C
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material
QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi..