Polymer Property : 100% Modulus = 0.00106 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00106 GPa
0.154 ksi
DCBP Cure
Shin-Etsu Silicones SV-14000U Silicone Rubber
SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..
100% Modulus 0.00106 GPa
0.154 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer
Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is..