Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00105 GPa | 0.152 ksi | ASTM D 412 |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.00105 GPa | 0.153 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
100% Modulus | 0.00105 GPa | 0.153 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6830 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |