Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000400 GPa | 0.0580 ksi | ISO 37 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |