Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 79.3 MPa | 11500 psi | Hydrostatic Crush Strength |
Engineered Syntactic Systems AZ-34 Deep Water Syntactic Foam Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c.. |