Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 26.2 MPa | 3800 psi | Hydrostatic Crush Strength |
Engineered Syntactic Systems MZ-24 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |