Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hydrostatic Design Basis = 1160 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hydrostatic Design Basis 8.00 MPa
1160 psi
MRS Classified; ISO 9080
SCG Chemicals EL-Leneâ„¢ H5211P High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Hydrostatic Design Basis 8.00 MPa
1160 psi
ISO 9080
SCG Chemicals EL-Leneâ„¢ H5211PC High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA, LNE, AENOR,..
Copyright © lookpolymers.com All Rights Reserved