Polymer Property : Hydrostatic Design Basis = 10.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hydrostatic Design Basis 10.0 MPa
1450 psi
MRS Classified; ISO 9080
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Hydrostatic Design Basis 10.0 MPa
1450 psi
ISO 9080
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi..
Hydrostatic Design Basis 10.0 MPa
1450 psi
ISO 9080
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA..