Mechanical Properties | Metric | English | Comments |
---|---|---|---|
PENT | >= 2000 hour @Temperature 80.0 °C |
>= 2000 hour @Temperature 176 °F |
2.4MPa |
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip.. |