Mechanical Properties | Metric | English | Comments |
---|---|---|---|
PENT | 200 hour | 200 hour | Compression molded parts prepared according to ASTM D 1928 Procedure C.; ASTM F1473 |
Dow DGDB-2480 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOLâ„¢ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su.. |