Mechanical Properties | Metric | English | Comments |
---|---|---|---|
PENT | >= 1500 hour @Temperature 80.0 °C |
>= 1500 hour @Temperature 176 °F |
2.4MPa |
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications in.. |