Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 9.80 J @Temperature 23.0 °C |
7.23 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 9.80 J @Temperature 23.0 °C |
7.23 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |