Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 12.2 J @Temperature 23.0 °C |
9.00 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |