Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 12.1 J @Thickness 102 mm |
8.92 ft-lb @Thickness 4.00 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Impact Test | 12.1 J @Temperature 23.0 °C |
8.92 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |