Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 9.49 J

@Temperature 23.0 °C
7.00 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin  (discontinued **)
OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou..