Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 92.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
67.9 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Impact Test | 92.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
67.9 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren.. |