Mechanical Properties Metric English Comments
Impact Test 8.20 J

@Temperature -30.0 °C
6.05 ft-lb

@Temperature -22.0 °F
ASTM D3763
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade
Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor..
Impact Test 8.20 J

@Temperature -40.0 °C
6.05 ft-lb

@Temperature -40.0 °F
ASTM D3763
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade
Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr..
Impact Test 8.20 J

@Temperature 23.0 °C
6.05 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..