Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |