Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Lexan® IP300 PC
Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America..
Impact Test 50.0 J

@Temperature -30.0 °C
36.9 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Lexan® IP300 PC
Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
Impact Test 50.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
36.9 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
Braskem RC35U4 LLDPE Rotomolding Polyethylene
The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te..
Impact Test 50.0 J

@Diameter 25.4 mm,
Temperature 150 °C
36.9 ft-lb

@Diameter 1.00 in,
Temperature 302 °F
310 HB.
Assab Steels 618 Plastic Mold Material
ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Assab Steels ASP 23 Cold Work Steel
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope..