Mechanical Properties Metric English Comments
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 358HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 925 Injection Molding Grade
Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties..
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
High speed instrumented impact (puncture); Energy @ max load; ASTM D3763
Diamond Polymers NPP 60-1010 PCTA Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Impact Test 42.0 J

@Diameter 25.4 mm,
Temperature 100 °C
31.0 ft-lb

@Diameter 1.00 in,
Temperature 212 °F
bar. 310 HB.
Assab Steels 618 Plastic Mold Material
ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu..