Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 28.0 J @Thickness 4.00 mm |
20.7 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Impact Test | 28.0 J @Thickness 4.00 mm |
20.7 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |
|||
Impact Test | 28.0 J @Thickness 4.00 mm |
20.7 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Impact Test | 28.0 J @Thickness 4.00 mm |
20.7 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 28.0 J @Thickness 4.00 mm |
20.7 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |