Polymer Property : Impact Test = 224 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 224 J

@Thickness 6.35 mm,
Temperature -40.0 °C
165 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM Impact
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren..