Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 16.3 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 16.3 J

@Temperature -40.0 °C
12.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin  (discontinued **)
OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou..
Impact Test 16.3 J

@Temperature 23.0 °C
12.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne..
Impact Test 16.3 J

@Temperature 23.0 °C
12.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Impact Test 16.3 J

@Temperature -17.8 °C
12.0 ft-lb

@Temperature 0.000 °F
Multiaxial Impact, Total Energy; CEAST
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade
Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams.