Mechanical Properties Metric English Comments
Impact Test 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
Instrumented, 2.2 m/s, ductile; ASTM 3763
Phillips Sumika Marlex® ABF-300 High Flow Thermoplastic Olefin  (discontinued **)
Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
Impact Test 21.0 J

@Temperature -30.0 °C
15.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 358HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 21.0 J

@Treatment Temp. 200 °C
15.5 ft-lb

@Treatment Temp. 392 °F
200°C Tempering temperature (2h + 2h)
Assab Steels 8407 SUPREME Hot Work Steel
8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and ..