Impact Test 15.5 J

@Temperature 300 °C
11.4 ft-lb

@Temperature 572 °F
Charpy-V specimens, transverse direction.
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..