Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 20.0 J @Temperature 0.000 °C |
14.8 ft-lb @Temperature 32.0 °F |
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763 |
S&E Specialty Polymers TufFill™ 5010UV Polyolefin Application: Thermoplastic polyolefin material is designed for automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or pai.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Multiaxial Impact (3.4 m/s, 40-mm ring, M831 Striker); Energy to Peak Load; ASTM-D3763 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Multi-Axial Impact, Fractovis J; Energy Max; ASTM-D3763 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Multiaxial Impact; E-max; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Impact Test | 20.0 J @Temperature 0.000 °C |
14.8 ft-lb @Temperature 32.0 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Impact Test | 20.0 J @Treatment Temp. 600 °C |
14.8 ft-lb @Treatment Temp. 1110 °F |
|
Assab Steels 8407 SUPREME Hot Work Steel 8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and .. |