Polymer Property : Izod Impact Unnotched = 95.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 129 J
95.0 ft-lb
Oil Quenched from 788°C; 538°C Temper Temperature
Latrobe Graph-Mo® Cold Work Tool Steel (ASTM O6)
Graph-Mo tool steel is an oil-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles wh..