Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 54.2 - 81.3 J @Diameter 30.5 mm |
40.0 - 60.0 ft-lb @Diameter 1.20 in |
bar |
Meehanite Almanite® W2 Wear and Abrasion Resisting Cast Iron Type W2 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W2 has a martensitic matrix.General Meehanite information - Meehanite metal .. |