Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact Unnotched = 67.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 90.8 J
67.0 ft-lb
Oil Quenched at 1163°C; 580°C Temper Temperature
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel
TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and its relatively low cost..
Copyright © lookpolymers.com All Rights Reserved