Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 59.7 J | 44.0 ft-lb | Oil Quenched at 1175°C; 594°C Temper Temperature |
Latrobe CM-52â„¢ ASTM M52 High Speed Steel CM-52 is classified as an intermediate type high speed steel of the molybdenum chromium-vanadium variety. It is recommended for intermediate cutting applications such as commercial twist drills and .. |
|||
Izod Impact Unnotched | 59.7 J | 44.0 ft-lb | Oil Quenched at 1218°C; 622°C Temper Temperature |
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |