Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 77.3 J | 57.0 ft-lb | Oil Quenched at 1163°C; 622°C Temper Temperature |
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and
its relatively low cost.. |