Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 47.0 J | 34.7 ft-lb | when tempered at 900°F |
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4) Carpenter Four Star, a molybdenum-tungsten high speed tool steel possessing high carbon and vanadium contents, provides a very high degree of wear resistance coupled with high strength.Applications:.. |