Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 4.00 J | 2.95 ft-lb | |
Kennametal Stellite Delcrome® 90 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and.. |