Polymer Property : Izod Impact Unnotched = 37.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 50.2 J
37.0 ft-lb
Oil Quenched at 1177°C; 482°C Temper Temperature
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel
CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge..