Mechanical Properties Metric English Comments
Izod Impact Unnotched 16.3 - 27.1 J

@Diameter 20.3 mm
12.0 - 20.0 ft-lb

@Diameter 0.798 in
Meehanite GC-40 Flake Graphite Cast Iron
Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d..