Polymer Property : Izod Impact Unnotched = 135.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 135.6 J
100.0 ft-lb
Longitudinal
Carpenter Micro-Melt® 9 Tough Treated Tool Steel
Micro-Melt® 9 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with goo..