Polymer Property : Izod Impact Unnotched = 122 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 122 J
90.0 ft-lb
Air Cooled from 954°C; 316°C Temper Temperature
Latrobe LSSâ„¢ A2 Tool Steel (ASTM A2)
TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance be..
Izod Impact Unnotched 122 J
90.0 ft-lb
Crucible Steel 410 Chromium Steel
Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci..