Polymer Property : Izod Impact Unnotched = 100 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 100 J
73.8 ft-lb
when tempered at 400°F
Carpenter No. 484® (Carpenter Air-Hard; AISI A2)
No. 484 tool steel is an air hardening steel capable of hardening throughout in heavy sections. It has been used for those applications in which the sections are very large and those involving extre..