Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 675 MPa | 97900 psi | ASTM C773 |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |