Polymer Property : Compressive Strength = 95000 psi
Polymer Property :
Compressive Strength =
95000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
655
MPa
95000
psi
McDanel Advanced Ceramics MV-20 Mullite
Information provided by McDanel Advanced Ceramic Technologies