Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 92.4 MPa | 13400 psi | Parallel |
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Compressive Strength | 92.4 MPa | 13400 psi | ASTM D695 |
Ensinger Tecatron® XP-65 Compression Molded PPS Compound, 30% Fiberglass with 15% PTFE Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Compressive Strength | 92.4 MPa | 13400 psi | |
Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many spe.. |
|||
Compressive Strength | 92.4 MPa | 13400 psi | |
Abatron AboCast 22-30/AboCure 50-4 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |