Polymer Property : Compressive Strength = 91400 psi
Polymer Property :
Compressive Strength =
91400 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
630
MPa
91400
psi
Longitudinal
Goodfellow Carbon/Polyetheretherketone (PEEK) Composite
Carbon Fiber - PEEK MatrixInformation provided by Goodfellow.