Mechanical Properties Metric English Comments
Compressive Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Compressive Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..
Compressive Strength 48.26 - 62.05 MPa
7000 - 9000 psi
after 816°C
Pyrotek Pyrocast ZS Refractory Shapes
Aggregate Base: Fused SilicaApplicationsTransfer troughs Information provided by Pyrotek.