Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 83.0 MPa | 12000 psi | |
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement Pyrocast FSC-2000 eliminates the need for cement pre-mixing or rolling while providing the same outstanding characteristics of all dense fused silica products.ApplicationsAdhesive Coating Patching c.. |
|||
Compressive Strength | 83.0 MPa | 12000 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 83.0 MPa @Strain 3.50 % |
12000 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |