Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 552 MPa | 80100 psi | |
Pyrotek TS-330 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Light Orange color. Very high compressive and flexural strength.Information provided by Pyrotek. |
|||
Compressive Strength | 552 MPa | 80100 psi | |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Compressive Strength | 552 MPa | 80100 psi | |
Du-Co Ceramics DC-9-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |