Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 78.0 MPa @Time 360000 sec |
11300 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Compressive Strength | 78.0 MPa | 11300 psi | |
Henkel Hysol EA 9380 Paste Adhesive System Cures at low temperature. Offers strength, toughness and high temperature resistance of heat-curing film adhesives, with greater flexibility and ease of use. Can be applied to large parts with contr.. |