Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | >= 760 MPa | >= 110000 psi | Ambient |
China-Yixing Longly Refractories Seggar SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |